STANDARDS
MECHANICAL PROPERTIES AT AMBIENT TEMPERATUREIN ANNEALED CONDITION
SURFACEFINISH
0.2% Proof strength
1% Proof strength
Tensile strength
Elongation %
Hardness
N/mm2
HB
HRB
EN 10088-2/2005
2B & 2R
240
420-600
23
ASTM A 240/SA 240
2B & BA
205
415
22
183
89
OTELINOX
2B
–
2R & BA
280 – 345
460-475
29-32